The placer gold ore washing operation

 

The placer gold ore washing operation includes three processes of crushing, screening and desliming. It is a very important and necessary operation before the placer gold ore is sorted. The reason why this operation is important is that it not only breaks and separates the mud and sand, but also removes the gold particles adhering to the surface of the gravel, and once a large amount of gold-free gravel can be screened out, it can be discarded directly; the general yield can be It reaches 40%-50% of the ore, and at the same time, most of the slime is removed.

In placer gold sorting, desliming, like removing large gravels, is also a very important preparatory operation. Materials less than 0.1mm in placer gold generally do not contain gold or contain very little gold. For example, gold less than 0.1mm in placer gold in Hunchun Gold Mine only accounts for 0.15%, while the same-sized ore slime accounts for 13.77% of the original ore sand. This kind of gold smaller than 0.1mm is commonly known as floating gold, which is difficult to recover during the sorting process.

In the placer gold ore dressing plant, always try to remove the slime less than 0.1mm in advance. Desliming equipment commonly used in production has desliming buckets of various specifications. However, the chute gold separation allows wide material particle size and large processing capacity, so the chute does not desilt before separation.

Comments

Popular posts from this blog

Chromite purification processing method

At present, chromium ores with industrial value are generally chromium-magnesia spinel or chromium-iron spinel minerals, which contain a large amount of chromium oxide, with a content of about 18% to 62%, and generally also contain metals such as aluminum and nickel. Its characteristics make the chromium ore beneficiation process present a rich and diverse state. Due to the properties of chromium, chromium ore beneficiation processes include gravity separation, magnetic separation, flotation, combined beneficiation, chemical beneficiation, etc. Commonly used in industry are single gravity separation, single magnetic separation, and gravity-magnetic combined beneficiation processes. In terms of equipment selection, shakers and jigs are mostly used in the gravity separation stage, while the equipment selection in the magnetic separation stage is determined based on the magnetism of the ore.

The classifications of quartz sand

  1. Ordinary quartz sand: The surface of ordinary quartz sand seems to have a layer of yellow skin, and some have large particles and strong fire resistance. It is a kind of quartz sand processed by the manufacturer after using natural quartz ore in the production process, such as washing and drying. No impurities can be seen in the quartz sand through the second water treatment filtration. It is the best choice for chemical water treatment. It can block the sundries suspended in the water and maintain the quality and beauty of the water. 2. Refined quartz sand: Refined quartz sand is a mineral made by the manufacturer after carefully selected quartz stone. According to different requirements of users, the range used is also different. But generally the main use of refined quartz sand is in glass products, because refined quartz sand is refractory and precision casting, especially suitable for fireproof glass materials.

Sandblasting nozzle classification and use

Using high-pressure air as a power source to drive abrasive particles to hit objects within a certain range will produce a great impact. The function of the sandblasting nozzle is to spray abrasive particles on the object evenly and efficiently. Sandblasting nozzles can be divided into: straight hole sandblasting nozzle, Venturi sandblasting nozzle , double Venturi sandblasting nozzle, angle sandblasting nozzle Straight hole nozzle: There are only contraction section and straight section inside, the structure is simple and easy to manufacture. This kind of nozzle cannot overcome the vortex phenomenon existing at the inlet end, and the pressure loss is large; the abrasive velocity at the outlet is less than 100m/s under the pressure of 0.7MPa.